Skip to main content

plastic molding term

plastic molding term


Heat-distortion temperature (°F) at fiber stress of 264 psi (ASTM D 648) is a statement of the temperature required to permit an arbitrary standard amount of deflection by a standard load, in a test in which the specimen is subjected to a gradually increasing temperature. It is thus an indication of the ability of a material to retain its stiffness, or resistance to deformation, against the weakening influence of high temperature. A similar test,under the lower load of 66 psi (ASTM D 648), in which, of course, a higher temperature is recorded, has similar significance for material subjected to lighter load. Values determined by this second test are shown, for some materials, in the 6th column of the table. A large difference between heat-distortion temperatures in these two tests gives warning of the need to pay particular attention to designing so as to minimize the stress in service of articles subjected to heat.

Impact strength, Izod {ft-lb per iti. of notch') (ASTM D 256) is the energy required to break a notched test bar by means of a sharp blow, and thus is indication of the shock-resistance of a material. A brittle or notch-sensitive material has low impact strength.

Tensile strength {psi) (ASTM D 638), i.e., the force required to break by simple tension, is seldom of direct significance in the choice of a plastic for a specific application, because usually the design is governed by the need to avoid distortion, which occurs under much lower stresses, but it may serve as a preliminary indication of the general mechanical strength of a plastic, and as a guide in applications which are primarily structural.

Recommended service temperature (°F) for molded articles subject to no stress cannot be stated in terms of any single definitive test. The values given in this column are based merely on general experience, and have no consistent relationship with respective heat-distortion temperatures under high and low loads. All three figures should be taken into account, and also, of course, the fact that continuous contact with water or chemicals may lower very much the temperature which a molded article can tolerate without distortion.

Heat-distortion temperature (°F) at fiber stress of 66 ps't (ASTM D 648) has been mentioned above, in connection with the companion test at 264 psi.

(Ma) Flexural strength (psi、(ASTM D 790) is a direct measure of the load required to cause failure by bending. Since usually a molded article must be designed to hold its shape under flexure, rather than merely not to break, a test for flexural stiffness, or for modulus of elasticity, is more generally significant than this one, but flexural strength is included here because it forms part of certain specifications for plastics.

(Mb) Compressive strength (psi) (ASTM D 695), the measure of compressive load required to cause failure, is seldom of direct significance for thermoplastic materials, since an article must usually be designed to resist deformation, which of course occurs under loads much less than that which will cause failure — and particularly so if the load is a permanent one, and large enough to cause cold flow, even though no immediate permanent distortion. Compressive strength, then, can serve usually only as a base to which to apply a large factor of safety.

(Me) Modulus of elasticity in tension (psi) (ASTM D 638) is a measure of the force required to produce a given change in dimension. Thus a high modulus is associated with rigidity and ability to hold shape under momentary loading. Under prolonged loading, however, deformation may develop in a plastic through cold flow; and under repeated loading through fatigue. The moduli of the plastics are low in comparison with those of structural metals.

(Md) Rockwell hardness (ASTM D 785) expresses resistance to penetration by brief contact with a heavily loaded small spherical bail, and thus measures one type of hardness. It is not to be interpreted as a measure of saatch-resistance.

(Me) Specific gravity (ASTM D 792) is usually important only as affecting the number of articles obtainable per unit weight of material.

(Ea, Eb, Ec) Dissipation factor at 60, 10s and 106 cycles per second (ASTM D 150) is a measure of the percentage of AC electrical energy lost as heat within a material used as a dielectric. A low dissipation factor is desirable in electrical insulation because it minimizes not only the waste of energy but also the immediate and cumulative effects of heat upon the material. On the other hand, a material of very low dissipation factor cannot be preheated or heat-sealed by high-frequency methods of heating.

(Ed, Ee, Ef) Dielectric constant (specific inductive capacity) at 60, 10z and 106 cycles per second (ASTM D 150) of a material is the ratio of the capacitance of a capacitor in which the material is the dielectric to the capacitance of the same capacitor with vacuum as the dielectric; thus, dielectric constant is directly a measure of the value of the material as dielectric in a capacitor.

(Eg, Eh) Dielectric strength short-time and step-by-step {volts per mil) (ASTM D 149) are measures of the voltage required to cause puncture, and thus are indicative of the thickness of insulation required to withstand a given voltage. (Actually, the thickness is usually more likely to be governed by mechanical considerations than by electrical.)

(Ei) Volume resistivity (megohm-cm) (ASTM D 257) is a measure of internal electrical resistance, i.e., resistance to steady passage of current through the material (not resistance to puncture), and thus a measure of suitability to serve as an insulator.

(Ej) Insulation resistance (megohms) (ASTM D 257) is a more realistic measure of insulating value, since it is calculated from the current passing both through the material and along its surface, and is determined on specimens conditioned at 50 per cent relative humidity.

(Ek) Arc-resistance (seconds) (ASTM D 495) is a measure of suitability for use under arcing conditions.

(Oa) Index of refraction (ASTM D 542) influences the ”brilliance” of a transparent plastic, determines the limit of curvature in a light-piping system, and is a necessary factor in the calculation of the shape of a lens or reflector.

(Ob) Light-/ransviissio;; (per cent、(ASTM D 791) is important in applications in optics and illumination.

(Oc) Haze (per cent) (ASTM D 1003) is a factor in the appearance of transparent plastics, and important in applications in optics and illumination.

(Ta) Coefficient of linear thermal expansion per °C (ASTM D 696) represents the magnitude of change in dimensions with change of temperature, which may be important in a device graduated for accurate measurement, or in an assembly of plastic with metal or other material, where differential expansion must be considered. Also it is a factor in the shrinkage of molded articles from the dimensions of the mold, and hence in the design of molds to yield articles of desired dimensions.

(Tb) Rate of burning {in. per minute) (ASTM D 635),i.e., the rate of propagation of flame in a test piece, is less important than the separation, by this test, of materials which when ignited will continue to burn and those which will not support combustion — i.e., are self-extinguishing.

(Ca) Water-absorption (per cent) (ASTM D 570) is usually important only because of the effects of absorbed water on other properties, e.g., impairment of electrical properties; swelling and warpage; impairment of rigidity; enhancement of toughness and impact strength.

(Aa) Weight loss (per cent) is a measure of the tendency of a plastic to lose weight upon aging, through evaporation of plasticizers or softeners. It is determined by weighing a specimen, heating it at 180 士 2°F for 72 hr, reweighing, and calculating the percentage loss in weight.

Comments

Popular posts from this blog

模具报价表 当前日期 产品名称 客户报价 利润点数(预设值13%) 汇率 报出价格(美元) 人民币价格 合计: $0.00 ¥0.00
高级包装体积重量报关计算器 (已修复) 高级包装体积重量计算器 (已修复) 使用说明: 本计算器用于同步计算包装的体积和重量。点击“添加项目行”可增加条目。 新功能: 1. 表头已冻结,可独立滚动数据。 2. 将鼠标悬停在表头列的右边缘可调整列宽。 3. 支持从Excel或网页表格直接粘贴多行多列数据。 4. 支持通过“导入Excel”按钮批量加载数据。 体积计算模块 项目名称 长 (cm) 宽 (cm) 高 (cm) 每箱体积 (m³) 每箱数量 箱数 总数量 总体积 (m³) 操作 添加项目行 导入Excel 清空数据 ...

injection molded lenses,injection molding optics

injection molded lenses,injection molding optics Injection molded lenses are an important part of many optical applications. At Topworks plastics, we offer a one-stop service for the design, tooling and injection molding of these lenses from China. We have years of experience in this field, and our team of experts can deliver high quality results quickly and efficiently. We offer a variety of different lens designs to suit your specific needs, and our flexible manufacturing process means that we can produce custom parts quickly and easily. Topworks plastics have extensive experience with this process and know how to get the best results from it. we can use their expertise to create custom pieces that fit your specifications perfectly. We offer fast turnaround times so that you can get what you need when you need it without having to wait around for weeks or months on end for your product to be completed. Topworks plastics also keep costs down by usi...